Title 037 · Title 37
Strength test.
Citation: N.D. Admin. Code § 37-02-01-10
Section: 37-02-01-10
37-02-01-10. Strength test. Each test sample shall be dropped from a height of five feet [1.53 meters] to a smooth, hard surface equivalent to rigid metal or concrete. Each test sample shall be submitted to three drop tests: 3 corner drop, edge drop, and flat drop. Failure shall be considered to have occurred when the emblem will no longer meet requirements in section 37-02-01-03. General Authority: NDCC 39-21-50 Law Implemented: NDCC 39-21-50 4